Treatment of API 650 low-alloy steel tanks welding defects:
1. Lack of fusion: once found, it should be shoveled and grinded off before re welding.
2. Incomplete penetration: over standard defects shall be removed and re welded. When welding on both sides, the shallow side of the groove can be grinded and shoveled to expose the welding root on one side, and then the welding is repaired.
3. Slag inclusion: over standard defects shall be removed and re welded.
4. Crater: weld to full after grinding.
5. Air hole: if the internal air hole exceeds the standard, it shall be welded again after being removed by grinding shovel, and the surface air hole shall be removed by grinding wheel and then repaired.

These API 650 documents will define the bases of design, operation, inspection, tests, examinations, and maintenance of an API 650 low-alloy steel tanks industrial facility. Bidders will study and analyze all this API 650 documentation, both during the preparation of the quotation and during the execution of each project activity.

The company has huge steel API 650 low-alloy steel tanks products stock all the year round to meet the urgent needs of customers. For stock products, we can arrange delivery within 3 days. The transportation department and shipping department shall coordinate and follow up to update the progress to customers regularly, i.e. where the goods have arrived, so as to let customers not worry and rest assured. Think about what the customers think and what the customers are anxious about, solve problems for customers efficiently and effectively, is the direction of our unremitting efforts.

Have a question? Get a Free Consultation

If you are interested in our storage tanks, you can get contact with us through online consulting, demand table submission, e-mails and telephones.

Corporate Office

High-Tech Development Zone, Zhengzhou, China

Contact us

+86-371-86151527
[email protected]

Send a Message!